Stir Bar Coatings and Cores: PTFE, Glass, Polypropylene and the 260 °C Limit
The same PTFE coating is rated 225 °C by one vendor, 260 °C by another and 290 °C in a coatings table. The span is 65 K for one material.
Equipment Hub / Measurement & glassware
Calibration weights, volumetric flasks, test sieves, thermocouples, stir bars, Karl Fischer reagents and drying media.
Parts covered: Calibration weights, Class A flasks, ASTM/ISO test sieves, thermocouples, PTFE stir bars, molecular sieves.
Choose the right part
The same PTFE coating is rated 225 °C by one vendor, 260 °C by another and 290 °C in a coatings table. The span is 65 K for one material.
Used PTFE bars have been found carrying palladium, platinum and iron in surface cracks, and a catalyst-free reaction stirred with one produced conversion.
THF from a sodium still came out at 43 ppm. THF standing over activated 3 Å sieves came out at 4.1 ppm in three days. The still had the reputation.
A compliant 150 µm sieve may contain individual openings up to 193 µm. Two sieves with the same label are not the same instrument.
The number on the bottle is a nominal strength. What the titrator needs is how many milligrams of water that bottle actually consumes per millilitre today.
A 10 mL Class A flask is allowed 0.20 % error and a 1 L one 0.03 %. The class letter alone does not tell you whether the flask matters in your method.
A Class 1 probe is allowed ±1.6 °C at 400 °C. The alloy can lose 1–2 °C of that by itself, just from sitting in a tempering oven through a shift.
At one kilogram, E2 allows ±1.6 mg and F2 allows ±16 mg. Each class step is about a factor of three, which is what you actually pay for.