Laboratory Filter Paper Grades: Retention, Flow Time and Ash
Grade 5 and Grade 42 are both rated 2.5 µm. Their listed filtration times are 1,420 and 1,870 seconds, and neither listing names the method behind the number.

Disclosure: We may earn a commission if you purchase through links on this page, at no additional cost to you. Our selection criteria do not depend on commission; see our affiliate disclosure.
Filter paper is one of the cheapest consumables on a bench, and it tends to be bought by whatever catalogue number the last order sheet carried. That works until a fine precipitate runs through the cone, or an ashing step leaves weight that should not be there. At that point the grade number stops being a detail.
This guide goes through what the grading systems actually measure, where the published numbers disagree with each other, and how to match a paper to a job. The figures come from two places: the ASTM E832 specification, seen through preview excerpts rather than the full licensed text, and distributor listings of Whatman papers, plus a distributor page and a Scribd copy of the manufacturer's own guide. Where those sources conflict, both values are shown rather than one being picked.
The two types in ASTM E832
ASTM E832 is the specification for laboratory filter papers. It sorts them into two types by purpose. Type I is for qualitative work and is described as low ash. Type II is for quantitative analysis and is described as ashless. Inside the types, papers are graded into classes by flow rate and by the sort of precipitate they must hold back. One small oddity: the abstract on the 2003 edition's preview page says "seven classes", but the body of the same edition lists eight, AA through G.
| Class | Type | Intended for | Max water flow time (s) | Filtrate must be clear of |
|---|---|---|---|---|
| AA | I | very coarse, gelatinous precipitates; very fast | 10 | ferric hydroxide |
| A | I | coarse, gelatinous; fast | 20 | ferric hydroxide |
| B | I | medium-size; medium flow | 40 | lead sulfate |
| C | I | fine; slow | 150 | barium sulfate |
| D | I | fine; slow; hardened so precipitate can be scraped off | 300 | barium sulfate |
| E | II | coarse, gelatinous; fast | 20 | ferric hydroxide |
| F | II | medium-size; medium flow | 40 | lead sulfate |
| G | II | fine; slow | 150 | barium sulfate |
The preview also carries a wet bursting strength column, but its layout was garbled in the copies available, so those numbers are not quoted.
Three details matter more than the table suggests. First, retention is defined by a chemical test, not a micron figure: the filtrate has to come through clear for a named precipitate. A paper that passes for ferric hydroxide, which is coarse and gelatinous, says nothing about whether it holds barium sulfate, and barium sulfate is the demanding one that sets the bar for the slow classes. Second, the Type II ash limit is 0.01 %, determined either by the standard's own muffle-furnace procedure or by TAPPI T413. That procedure heats the specimen to about 925 °C, holds it for 2 hours, and calls ignition complete when the covered crucible and ash change by no more than 0.2 mg after a further 30 minutes at that temperature. Third, Class D is the only class defined by surface: it must be hard enough that collected precipitate can be scraped off the sheet.
What a micron rating tells you, and what it does not
Manufacturers rarely publish ASTM class letters. None of the listings read for this article gave one. They publish a micron figure instead, usually called particle retention, sometimes pore size. Those two systems do not translate into each other, and the micron figures are softer than they look.
Start with how the same paper is described in different places. Grade 1 is given as ">11 µm" particle retention on one distributor's pages but as "pore size: 11 µm" on a page that lists the same grade. Grade 2 is ">8 µm" on one and "8 µm" on the other. Grade 4 shows a particle retention of 25 µm and a pore size of "20 to 25 µm" in the same entry, while the other page gives 20–25 µm. Grade 41 is 20 µm on one and 20–25 µm on the other. The paper is the same in each case; the summaries differ in rounding and in the word used for the measurement.
A second problem sits underneath. For filter media in general, a Gusmer technical note discussing EMD Millipore's rating practice says that there are no industry standard guidelines for how pore size, retention or rating is determined, and that a nominal filter may not retain well at its stated size. The one paper maker found that defines its own number, MTC USA for its cellulose filter paper, says retention is the nominal retention of particulate at 98 % efficiency in liquid. The equivalent definition for Whatman's figures was not published in anything read for this article. So treat "11 µm" as a rating on one maker's scale, and expect that a paper from another brand with the same number may catch more or less.
One pair shows how little the rating alone tells you. Grade 5, a qualitative paper, and Grade 42, a quantitative ashless one, are both listed at 2.5 µm. Their listed filtration speeds are 1,420 s and 1,870 s, with no method named for either. Same retention number, about a third longer wait.
Flow time: two methods and no fixed conversion
Speed is the other number on a listing, and it hides a trap. ASTM E832 allows the flow rate to be determined by its own test, or by the Herzberg method. Some listings show both values. Grade 54, a hardened low-ash paper, shows 10 seconds by ASTM and 39 by Herzberg. Grade 40 shows 75 and 340. Grade 542, hardened ashless, shows 250 and 2,510. The ratios work out at roughly 3.9, 4.5 and 10. There is no single factor that turns one scale into the other, and the gap widens for the slower, finer papers.
That has two consequences. A speed quoted without its method, such as Grade 1 at 150 seconds or Grade 2 at 240, cannot be checked against the ASTM class limits. And ordering a "faster" substitute from another brand by comparing the speed lines alone is a gamble unless both lines name the same method.
There is one internal consistency check that does work. The manufacturer describes Grade 6 as filtering twice as fast as Grade 5. The listed times, 715 s (Herzberg, per the listing) against 1,420 s, do come out at almost exactly two to one, which suggests the unlabelled Grade 5 figure is also a Herzberg time. That is an inference, not something the page states.
One piece of arithmetic, which is arithmetic and not a manufacturer's claim: Grade 40 at 75 seconds by the ASTM test would miss the 40-second ceiling of Class F and sit under the 150-second ceiling of Class G, even though Grade 40 is sold as a medium-speed paper with 8 µm retention. No published assignment of a class to that grade turned up, so it is worth reading only as a warning that the micron label and the class system describe different things.
Ash, and why it rarely matters as much as people fear
The manufacturer's guide copy gives the ash limits for its quantitative families: a maximum of 0.007 % for Grades 40 to 44, 0.01 % for the 589 grades, and 0.006 % for hardened ashless papers. A hardened low-ash family, Grade 54 among them, sits between ashless and ordinary qualitative papers.
Those percentages look tiny, and in most weighing they are. Grade 1 is listed at a basis weight of 87 g/m². An 11 cm circle has an area of about 95 cm², or 0.0095 m², so it weighs close to 0.83 g. That uses Grade 1's weight only as a stand-in for a paper of similar substance; check the real weight on your own packet. At 0.007 % that circle leaves about 0.058 mg of ash, and at 0.01 % about 0.083 mg. Both are under the 0.1 mg readability the ASTM procedure itself uses. On a 0.1 mg balance, ashless paper residue effectively cannot be seen. On a 0.01 mg balance it is five to eight readout steps, and only then does the ash limit start to show up in the result.
The same sums show why the test is hard to run. The standard wants specimens of at least 6 g. At the 0.01 % limit that is 0.6 mg of ash, measured on a balance reading to 0.1 mg, so the check resolves roughly one sixth of the limit. That is adequate for acceptance testing, and a reason to be sceptical of ash quoted to many decimal places.
Hardening is a separate property from ash, though the two often arrive together. One listing describes Grade 541 as acid-hardened cellulose that reduces ash to an extremely low level, and the guide copy credits hardened ashless papers with high wet strength and chemical resistance. In practice that means a hardened paper survives vacuum filtration and acidic filtrates better. The trade-off shows in flow time: Grade 541 is listed at 22 µm, while Grade 542, listed at 2.7 µm, takes 250 seconds by the ASTM test. One listing puts 542 in gravimetric metal determinations and hydroxide collection, and Grade 41 in sample prep for metals after nitric acid digestion.
Matching the paper to the job
The listings give a stated application for most grades, and those descriptions are the most usable part of them. Grade 4 is described for air pollution monitoring where high flow matters and fine particle collection is not critical. Grade 5 is described as a clarifying filter for cloudy suspensions, water and soil work. Grade 6 is listed for boiler water analysis. Grade 3 is described as twice the thickness of Grade 1 (390 µm against 180 µm) for high precipitate capacity. Grade 589/3 is listed for ash-free dry mass of fine particulate such as insoluble material in fats or oils, and Grade 589/2 for medium-fine precipitates where the paper must be ashed.
From those, here are rules of thumb built on the sources above, and not published guidance.
If the work is gravimetric, where the paper goes into a furnace or the precipitate is weighed, start from Type II or the equivalent ashless family, then pick fineness from the precipitate. Barium sulfate and similar fine crystals point to the slow, fine end: Class G in ASTM terms, or something like Grade 42 or 542 among the common grades. Gelatinous hydroxides do the opposite. They blind a fine paper quickly, so a faster paper such as Grade 41 keeps the run moving. One distributor's text does put Grade 542 on hydroxide collection, which cuts the other way; the ASTM pairing of ferric hydroxide with the fast classes is the better starting point, and the test decides.
If the work is clarifying or routine cleanup, where nothing is weighed, a qualitative paper is enough and ash is irrelevant. Grade 1 as a default is defensible. Move to a Grade 5 or 6 when the filtrate is still cloudy, and to a Grade 4 or 113V when speed matters more than clarity.
If the filtrate is acidic, or filtration runs under vacuum, favour a hardened paper before you favour a finer one.
If you have to swap brands, match the retention figure and the named flow-time method first. Then borrow the idea behind E832's own retention test, which asks for nothing more than a clear filtrate for a named precipitate, and try it on your material.
Equipvia may earn a commission from qualifying purchases through this link. The link resolved to Product ID 1600165608777 during review. CPS resolution does not verify the seller's technical claims, the grade's equivalence, affiliate eligibility, or commission attribution. Check the actual selected variant and current terms before ordering.
This listing is a good illustration of the problem the rest of the page describes. It uses the grade 40 to 43 numbers as a selling label, but the brand field names a different manufacturer, and the paper is cotton linters in an unstated grade structure. A grade number borrowed from another maker's catalogue is a description of what the seller intends, not evidence that the retention, flow time or ash matches. If a method names a grade number, ask for the ash figure, the retention basis and the flow-time method for the actual paper being quoted.
A quick retention check, and the symptoms worth reading
The standard's retention section calls for 60° glass funnels with stems about 6 in. long. A bench version is cruder. Filter a representative charge, then run the filtrate through a second paper of the same grade and hold the two beside each other against a dark card. If the second is clear and the first was not, the first paper let solids by. If haze survives both, the grade is too open and needs to step toward something like Grade 5 or 42. Cloudiness in only the first few millilitres may just mean the paper had not bedded in. This is a qualitative reading, not a method.
Slow runs deserve a second look before anyone blames the paper. Grade 42 is listed at 1,870 s, and it is meant to be slow; a gelatinous hydroxide on it will crawl further, and the fix is a faster grade, not more patience. A cone that tears under vacuum wanted one of the hardened papers, since the guide copy credits them with high wet strength. Weights that will not repeat between runs may trace to fibres lifted when precipitate is scraped from a soft paper, the job Class D was specified for. Ash above the blank after furnace work usually means a qualitative paper sat where a Type II belonged.
Limits of the sources
The E832 class table rests on preview excerpts, so the bursting-strength limits are missing. The grade figures come from retailers and a copy of the manufacturer's guide, not from a current datasheet. For a written method or a purchasing specification, get the E832 text from ASTM and the datasheet for the exact grade.
Share this article