Borosilicate 3.3, Soda-Lime or Quartz: ISO 3585 Limits and Thermal Shock
A beaker, a pipette and a furnace tube can all be called glass and sit an order of magnitude apart in how they treat a hotplate.

Disclosure: We may earn a commission if you purchase through links on this page, at no additional cost to you. Our selection criteria do not depend on commission; see our affiliate disclosure.
John Morris Group's comparison table lists thermal expansion at 3.3 × 10⁻⁶ K⁻¹ for borosilicate 3.3, about 9.0 × 10⁻⁶ for soda-lime and about 0.5 × 10⁻⁶ for fused silica, with maximum working temperatures of about 500 °C, about 250 °C and above 1,000 °C. A beaker, a pipette and a furnace tube can therefore all be called glass and still sit an order of magnitude apart in how they treat a hotplate. The sources also disagree on how much temperature difference each glass survives, and this guide shows the disagreement instead of picking a winner.
The three materials, in figures
Borosilicate 3.3. Wikipedia gives the lab composition as roughly 80 percent silica and 13 percent boric oxide, a density of 2.23 g/cm³ and a mean specific heat of 0.83 J/(g·K) between 20 and 100 °C. John Morris puts its softening point at 820 °C. Saillart, a glassblower, lists DURAN with a transformation temperature of 525 °C and a density of 2.23.
Soda-lime. Conduct Science lists a thermal coefficient of expansion of 8.6 × 10⁻⁶ per °C between 0 and 300 °C, a softening point of 726 °C, an annealing range of 546 °C and a strain point of 514 °C. It adds that soda-lime is the cheapest laboratory glass to make and is usually what pipettes are made of.
Quartz. Conduct Science gives about 5.0 × 10⁻⁷ and John Morris about 0.5 × 10⁻⁶, and LIMS Wiki describes fused quartz as one-fifteenth the expansion of soda-lime. Machined Quartz lists a refractive index of 1.473 at 587.6 nm, a dielectric strength of 30 kV/mm, a volume resistance of 10¹⁵ Ω·cm and a stress-optical coefficient of 4.0 × 10⁻⁶ mm²/N. Wikipedia lists tube furnace liners and UV cuvettes among its uses.
Where the sources disagree on thermal shock
Wikipedia lists thermal shock tolerance of 330 °F (170 °C) for borosilicate and 100 °F (40 °C) for soda-lime, while a Wikipedia mirror lists 37 °C (99 °F) for soda-lime. John Morris lists up to 166 °C for borosilicate 3.3. Saillart lists ΔT = 100 K for DURAN and adds that wall thickness and product geometry influence it. ISO 718 is the thermal shock test method, known here by title only.
Those numbers are not interchangeable, and part of the reason is units. Reading Wikipedia's 330 °F and 170 °C as a pair, 330 °F is 165.6 °C as a reading but 183 K as a difference, and 100 °F is 37.8 °C as a reading but 56 K as a difference. A shock rating quoted in kelvin is a temperature difference; one quoted in degrees Celsius from a Fahrenheit source may be either. Treating 100 K as the working limit for a flask is a judgment, not a published rule, and it sits inside the range the sources give.
Maximum temperature, and the same unit problem
Wikipedia lists a maximum of about 500 °C, DWK about 500 °C for short periods, John Morris about 500 °C for borosilicate and about 250 °C for soda-lime, and Avantor's VitraPOR sheet gives 515 °C as the strain point and safe maximum with deformation danger at 580 °C. John Morris lists soda-lime expansion at about 9.0 × 10⁻⁶; Conduct Science lists 8.6 × 10⁻⁶ at 0 to 300 °C, plus a second table of 5.0 × 10⁻⁶ for an unnamed glass with a softening point of 786 °C and a density of 2.37.
Conversions for the limits above: 250 °C is 482 °F, 500 °C is 932 °F, 515 °C is 959 °F, 580 °C is 1,076 °F, 820 °C is 1,508 °F, 1,000 °C is 1,832 °F, and in absolute terms 250 °C is 523 K, 500 °C is 773 K, 515 °C is 788 K, 580 °C is 853 K, 820 °C is 1,093 K and 1,000 °C is 1,273 K. Conduct Science's 726 °C soda-lime softening point is its own quoted 1,340 °F, which is 1,339 °F by conversion, and its strain, annealing and softening points of 514, 546 and 726 °C are 957, 1,015 and 1,339 °F. Saillart's transformation point of 525 °C is 977 °F. Avantor's 65 K gap between 515 and 580 °C is 117 °F.
DWK adds that soda-lime melts at around 1,000 °C, which sits beside John Morris's 250 °C working maximum for the same glass. Melting and working temperature are different quantities, and a catalogue that lists only one of them invites the confusion.
What the expansion numbers mean in millimetres
Linear expansion is the coefficient times length times temperature rise. A 1 m rod heated by 100 K grows 0.33 mm in borosilicate 3.3, 0.90 mm in soda-lime at 9.0 × 10⁻⁶, and 0.05 mm in fused silica at 0.5 × 10⁻⁶. Heated by 300 K, the same rod grows 0.99 mm, 2.7 mm and 0.15 mm. Saillart makes the same point from the stress side: for a 1 K change, DURAN changes by 3.3 × 10⁻⁶ in relative length, which keeps strain low where a thermal gradient exists.
Two worked examples with the same coefficients. A 24 mm ground joint heated by 200 K widens by 0.016 mm in borosilicate 3.3, 0.043 mm in soda-lime at 9.0 × 10⁻⁶ and 0.002 mm in fused silica, so a borosilicate stopper in a soda-lime socket would open a mismatch of about 0.027 mm over that rise. For glass-to-metal seals, a 100 mm seal heated by 300 K shows a mismatch of 0.021 mm between 3.3 glass and a 4.0 tungsten-matched glass, 0.039 mm against Wikipedia's 4.6 molybdenum glass and 0.051 mm against a 5.0 Kovar-matched glass. All of these are arithmetic from published coefficients, not measured fits.
The ratios behind the common claim: 9.0 / 3.3 = 2.7 and 8.6 / 3.3 = 2.6, consistent with the "one-third" that Wikipedia and John Morris state. For fused silica, 3.3 / 0.5 = 6.6 and 9.0 / 0.5 = 18, against LIMS Wiki's one-fifteenth. The shock figures of 100 K and 170 K differ by a factor of 1.7.
What ISO 3585 requires
ISO 3585 defines "borosilicate glass 3.3" for laboratory glassware, glass plant, pipeline and fittings. The 1998 text is the third edition and cancels ISO 3585:1991, which itself revised a 1976 first edition. BSI lists the standard as current and under review and sells it for €152.15 excluding VAT, or about €5.43 for each year since publication to 2026.
ISO 3585:1998 lists hydrolytic grain class ISO 719-HGB 1 at 98 °C, ISO 720-HGA 1 at 121 °C and alkali class ISO 695-A2 or better. DWK lists acid class S1 under DIN 12116, compliance with DIN 12217 and ISO 1776 as a related method, and ASTM E438 Type 1 Class A and B for borosilicate. Avantor lists HGB 1, HGA 1 and S1, plus pharmaceutical Class I and Type I under the German and European pharmacopoeias and USP XXIII. DWK says alkaline solutions attack all glasses, with borosilicate moderately resistant at class A2, and says steam sterilisation can leach sodium ions. LIMS Wiki says borosilicate is slightly more expensive than soda-lime.
Neighbouring standards that come up when you read the reference lists: ISO 4803:1978 for borosilicate tubing, ISO 4797:2015 for boiling flasks with conical ground joints, ISO 3587:1976 for glass plant pipeline of nominal bore 15 to 150 mm, ISO 7884-1:1987 for viscosity and viscometric fixed points, and ISO 4802-1 and -2:1988 for hydrolytic resistance of interior surfaces. ISO 12775 refers to ISO 719, 720, 4802-1 and 4802-2 for hydrolytic resistance.
A property sheet from three pages
Conduct Science lists borosilicate 3.3 at a refractive index of 1.474, a dielectric constant of 4.6 at 1 MHz, a specific heat of 750 J/kg·°C and a thermal conductivity of 1.14 W/m·°C. Wikipedia gives 0.83 J/(g·K), which is 830 J/kg·K and sits above Conduct Science's 750 because the two quote different temperature ranges, 20 to 100 °C and 20 °C. On the same conversions, 0.83 J/(g·K) is 0.198 cal/(g·K) and 750 J/(kg·K) is 0.179 cal/(g·K), 1.14 W/(m·K) is 0.659 Btu/(h·ft·°F), and 30 kV/mm is 762 V per mil. Stress-optical coefficient 4.0 × 10⁻⁶ mm²/N equals 4.0 Brewster, and 10¹⁵ Ω·cm equals 10¹³ Ω·m.
Wikipedia calls the family crown glasses with Abbe numbers around 65 and refractive indices of 1.51 to 1.54, which is a broader family than the 3.3 grade. Conduct Science's 1.474 for one glass and Machined Quartz's 1.473 for quartz differ by 0.001, or 0.07 percent. Densities of 2.23, 2.34, 2.42, 2.37 and 2.53 g/cm³ are 139.2, 146.1, 151.1, 147.9 and 157.9 lb/ft³, and Conduct Science's specific gravity of 2.53 is 13.5 percent above 2.23.
Grades inside the borosilicate family
John Morris tabulates three grades. Grade 3.3 has 13.0 percent boron oxide, expansion 3.3, softening point 820 °C and density 2.23 g/cm³. Grade 4.9 has 10.5 percent, 4.9, 785 °C and 2.34. Grade 5.4 has 7.5 percent, 5.4, 770 °C and 2.42. Saillart lists FIOLAX at 4.9, transformation 565 °C and density 2.34, which matches John Morris on the two figures the pages share, expansion and density.
The lesson is that "borosilicate" is a family. Wikipedia says different borosilicates cover a range of expansions so they can seal to molybdenum at 4.6, tungsten at about 4.0 and Kovar at about 5.0. Only 3.3 is the grade ISO 3585 describes. The grade table shows expansion rising 1.48 and 1.64 times the 3.3 value, softening point falling by 35 °C and then 50 °C from 820 °C, and density rising 4.9 and 8.5 percent. Wikipedia's sealing glasses at 4.0 and 4.6 fall between grades 3.3 and 4.9, and the 5.0 Kovar match falls between 4.9 and 5.4.
The brand question follows from that. John Morris states that Corning distinguishes PYREX in capitals, its laboratory borosilicate 3.3 brand, from lowercase pyrex, consumer cookware now made from tempered soda-lime in some markets including the United States. Wikipedia says the European Pyrex maker Arc International uses borosilicate in its kitchen products, while the US kitchenware maker uses tempered soda-lime, and lists Pyrex, Bomex, Duran, TGI and Simax as names that refer to borosilicate when used for laboratory glassware.
Equipvia may earn a commission from qualifying purchases through this link. The link resolved to Product ID 1600101726031 during review. CPS resolution does not verify the seller's technical claims, the glass grade, affiliate eligibility, or commission attribution. Check the actual selected variant and current terms before ordering.
"Borosilicate 3.3" in a title is a grade claim, and on this page the grade is exactly what is being bought: 3.3 rather than 4.9 or 5.4, and a glass that passes HGB 1 rather than an unclassified one. Ask for the expansion coefficient on the certificate, the hydrolytic class at 98 °C, and whether the item was annealed after forming, since stresses left in the wall are what a thermal shock finds first. A beaker at one and a half dollars may well be the right grade; the point is that the price does not tell you, and the certificate does.
Choosing by the job
Specify "borosilicate 3.3 per ISO 3585" on the purchase order, not a brand name. For heat and freezer-to-bench work, borosilicate 3.3 is the default; soda-lime belongs in low-heat disposables; quartz comes out above 500 °C or for deep UV. That division is judgment, built on the figures above.
The supporting observations are scattered but consistent. John Morris says soda-lime flasks on hotplates commonly crack, and Wikipedia says soda-lime shatters when boiling water meets ice, which is the 40 °C shock figure in practice. Conduct Science lists soda-lime as the cheapest and common for pipettes, where thermal shock is not part of the job. Wikipedia lists UV cuvettes and furnace liners for quartz. Saillart lists amber DURAN at under 10 percent transmission between 300 and 500 nm, which is an absorbance above 1.0 since A = −log10(0.10) = 1.00, and John Morris lists actinic glass for light-sensitive pharmaceutical, biochemistry and environmental work.
What this article could not check
Section 5 of ISO 3585:1998 was not read, nor were the test methods behind the shock figures in the secondary sources. ASTM E438, DIN 12116 and DIN 12217 are known through manufacturer tables only, and ISO 718 by title. The conversion arithmetic throughout is arithmetic on published coefficients, not measurement. The 100 K working limit for a flask is a recommendation, not a standard.
Share this article